Alloy

Colmonoy 226

Alloy Type

Fuseweld Alloy

Nominal Composition (%)

B 0.80
Si 2.20

P 1.90
Ni Balance

Rockwell Hardness
(C-scale)

16-21

Density (gm/cc)

8.58

Fusing Temperature (approx.)

1715°F
935°C

Resistance:

to
Abrasion

to

Corrosion

to
Impact

to
Galling

 

6

2

1

3

Supplied Forms

Atomized Powder

Method of application

Fusewelder

Description and General Uses

 

Patented alloys specially designed for glass container mould protection and restoration. Also used for rebuilding automotive parts (clutch components).