Alloy |
Colmonoy 227 |
 |
|
Alloy Type |
Fuseweld Alloy |
|
Nominal Composition (%) |
B 0.90
Si 2.70 |
P 2.10
Ni Balance |
|
Rockwell Hardness
(C-scale) |
22-27 |
|
Density (gm/cc) |
8.53 |
|
Fusing Temperature (approx.) |
1680°F
915°C |
|
Resistance: |
to
Abrasion |
to
Corrosion |
to
Impact |
to
Galling |
|
|
6 |
2 |
1 |
3 |
|
Supplied Forms |
Atomized
Powder, Bare Rod |
|
Method of application |
Fusewelder,
Oxyacetylene, GTAW |
|
Description and General Uses
|
Patented
alloys specially designed for glass container mold protection and
restoration. Also used for rebuilding automotive parts (clutch
components). |