Alloy |
Colmonoy 42 |
 |
|
Alloy Type |
Nickel with Chromium Carbide |
|
Nominal Composition (%) |
C
0.20
Si 2.80
Cr 4.00 |
Fe 0.30
B 1.20
Mo 3.00
Ni Balance |
|
Rockwell Hardness
(C-scale) |
35-40 |
|
Density (gm/cc) |
8.50 |
|
Fusing Temperature (approx.) |
1800°F
980°C |
|
Resistance: |
to
Abrasion |
to
Corrosion |
to
Impact |
to
Galling |
|
|
4 |
2 |
2 |
3 |
|
Supplied Forms |
Atomized powder |
|
Method of application |
Spraywelder (42SA),
HVOF (43HV),
5P (42M) |
|
Description and General Uses
|
Better ductility and toughness than Colmonoy No. 52. Less hardness and
slightly less abrasion resistance. Finished by carbide tools and grinding.
|