Alloy |
Colmonoy 5 |
 |
|
Alloy Type |
Nickel with Chromium Boride |
|
Nominal Composition (%) |
C
0.50
Si 3.40
Cr 13.80 |
Fe 4.80
B 2.30
Ni Balance |
|
Rockwell Hardness
(C-scale) |
45-50 |
|
Density (gm/cc) |
8.24 |
|
Fusing Temperature (approx.) |
1880°F
1025°C |
|
Resistance: |
to
Abrasion |
to
Corrosion |
to
Impact |
to
Galling |
|
|
3 |
2 |
3 |
3 |
|
Supplied Forms |
Crushed Powder, Bare Rods, Ingot |
|
Method of application |
Spraywelder, Oxyacetylene, GTAW, PTA |
|
Description and General Uses
|
Has greater impact resistance and workability than Colmonoy No. 6. For
wear rings, plungers, dies. Finished with carbide tools and
grinding. See spec. II. |