Alloy
Wallex 55
Alloy Type
Cobalt Alloys
Nominal Composition (%)
C 2.30 Si 1.70 Cr 12.00
Rockwell Hardness (C-scale)
58 min.
Density (gm/cc)
11.90
Fusing Temperature (approx.)
2030°F 1110°C
Resistance:
to Abrasion
to
Corrosion
to Impact
to Galling
1
2
4
Supplied Forms
Composite Powder
Method of application
Spraywelder
Description and General Uses
Uses a cobalt-nickel matrix alloy to hold extremely hard tungsten-carbide particles. Primarily to protect surfaces against severe sliding abrasion. Finished by grinding.