Alloy |
Colmonoy 56 |
 |
|
Alloy Type |
Nickel with Chromium Boride |
|
Nominal Composition (%) |
C
0.60
Si 3.80
Cr 13.20 |
Fe 4.40
B 2.60
Ni Balance |
|
Rockwell Hardness
(C-scale) |
56-61 |
|
Density (gm/cc) |
8.18 |
|
Fusing Temperature (approx.) |
1885°F
1030°C |
|
Resistance: |
to
Abrasion |
to
Corrosion |
to
Impact |
to
Galling |
|
|
2 |
2 |
4 |
2 |
|
Supplied Forms |
Crushed Powder, Bare Rods, Ingot, Cored Wire |
|
Method of application |
Spraywelder, Oxyacetylene, GTAW, GMAW, PTA |
|
Description and General Uses
|
Better ductility and impact resistance than Colmonoy No. 6. Finished with
carbide tools and grinding. |