Alloy |
Colmonoy 6 |
 |
|
Alloy Type |
Nickel with Chromium Boride |
|
Nominal Composition (%) |
C
0.70
Si 4.20
Cr 14.30 |
Fe 4.00
B 3.00
Ni Balance |
|
Rockwell Hardness
(C-scale) |
56-61 |
|
Density (gm/cc) |
8.10 |
|
Fusing Temperature (approx.) |
1890°F
1030°C |
|
Resistance: |
to
Abrasion |
to
Corrosion |
to
Impact |
to
Galling |
|
|
1 |
1 |
4 |
1 |
|
Supplied Forms |
Crushed Powder, Bare Rods, Ingots |
|
Method of application |
Spraywelder, Oxyacetylene, GTAW, PTA, |
|
Description and General Uses
|
The
original, nickel-base hard-surfacing alloy, containing diamond-like
chromium borides (and carbides). Extremely resistant to wear, especially
under corrosive conditions. Low coefficient-of-friction. Can be
hot-formed. Finished by
grinding. See spec 1. |