Alloy

Colmonoy 62SM

Alloy Type

Nickel with Chromium Carbide

Nominal Composition (%)

C 0.70
Si 4.00

Cr 14.50

Fe 4.00
B 3.10
Ni Balance

Rockwell Hardness
(C-scale)

57-62

Density (gm/cc)

8.05

Fusing Temperature (approx.)

1875°F
1025°C

Resistance:

to
Abrasion

to

Corrosion

to
Impact

to
Galling

 

1

1

4

1

Supplied Forms

Atomized powder

Method of application

Spraywelder

5P

Description and General Uses

 

Recommended for hardfacing parts to resist wear, corrosion, heat and galling. Typical applications: shafts, sleeves, pump plungers, sucker rod couplings, bed knives, camshafts, bushings, mill guides, mixer blades, seal rings, brick manufacturing equipment, and conveyor screws. Finished by carbide tools and grinding