Alloy |
Colmonoy 72 |
 |
|
Alloy Type |
Nickel with Chromium Carbide |
|
Nominal Composition (%) |
C
0.50
Si 3.00
Cr 12.00
Fe 4.00 |
B 3.20
W 13.00
Ni Balance |
|
Rockwell Hardness
(C-scale) |
57-62 |
|
Density (gm/cc) |
9.51 |
|
Fusing Temperature (approx.) |
1940°F
1060°C |
|
Resistance: |
to
Abrasion |
to
Corrosion |
to
Impact |
to
Galling |
|
|
1 |
1 |
4 |
1 |
|
Supplied Forms |
Atomized Powder, Bare Rods, Ingot |
|
Method of application |
Spraywelder, Fusewelder, Oxyacetylene, GTAW |
|
Description and General Uses
|
Tungsten
content strengthens the nickel matrix, giving this alloy excellent
resistance to low-stress abrasion and scouring action. Wear
resistance often superior to Colmonoy No. 6 For pump parts. Finished by
grinding. |